The effectiveness of atmosphere during injection casting changes in the order of O2 > Air > N2 > Ar > He for Fe76Si9B10P5 bulk glassy alloy and 105 Pa He > 105 Pa Ar > 103 Pa Ar > vacuum for Zr65Al7.5Ni10Cu17.5−xPdx (x = 0–17.5 %) bulk glassy alloys.
pp 1131-1136